Solvent Popping In Paint

For automotive refinishers, there is nothing more frustrating than finishing defects. They can cause rework, create production bottlenecks and negatively impact a body shop’s bottom line.

Most finishing defects are the result of technician error or contaminants entering the spray booth, typically during the painting or drying process. While most finishing defects are preventable, correcting them can result in hours of additional labor and hundreds of dollars in unnecessary materials and expenses.

Here are four of the most common finishing defects in automotive refinishing, along with ways you can fix them and prevent them from happening:

One of the primary causes of finishing defects is dust and dirt in the basecoat or clearcoat. This is the result of contaminants entering the paint booth ā€” either through the air, from the painter’s attire or on items being painted (due to improper cleaning of a vehicle or parts).

When dirt settles in the wet film of the basecoat, it looks like a smattering of pinhole-sized specks. The dirt particles must be sanded out before reapplying basecoat to the affected areas.

During the application of clearcoat, when dirt is trapped in the wet film, it resembles little, bubble-like pimples. Since sanding and polishing only removes dirt on the surface of the clearcoat, reapplication of the basecoat and clearcoat is often required.

If the contamination is on the surface, buffing can typically remove it, although it is time-consuming. If the contamination is beneath the surface or is severe, the entire panel must be refinished.

Regularly cleaning your paint booth helps prevent dust and dirt from lingering in the booth. All crevices of the booth should be blown out to keep contaminants from becoming trapped. Painters should also wear lint-free spray suits, so they do not unknowingly carry dirt into their paint jobs.

Solvent popping occurs when trapped solvent expands and breaks through the applied paint film. Several problems can cause solvent popping, including:

  • Incorrect spraying viscosity, spraying pressure, flash-off times or drying timesĀ that result in solvents or air trapped in the film, leaving pop marks as it escapes
  • Insufficient drying of primer, mainly in the corners and edges
  • Film build is tooĀ thick
  • Incorrect selection of hardeners and thinners
  • Improper spraying techniques

If the solvent popping is on the surface ā€” also known as micro-popping ā€” sanding and buffing can sometimes remove it. If the solvent popping is beneath the surface, the entire finished area must be sanded, primed and repainted.

Applying a normal film thickness can help prevent solvent popping. It is best to follow the recommendations on the technical data sheet (TDS) from your paint supplier.

Edge mapping results from solvents in topcoats penetrating through areas of the undercoats; it resembles a wrinkling around the area that has been repaired. Edge mapping is caused by one of the following situations:

  • Filler/primer isĀ not fully cured before top-coating
  • Topcoat is sanded through to the substrate
  • Unsuitable filler/primer is used
  • Filler/primer isĀ applied incorrectly

To fix edge mapping, the topcoat must dry thoroughly. Then, the damaged area must be sanded, isolated and repainted.

Edge mapping can be avoided by not sanding through to soft substrates, which can be identified by conducting a solvent test. You should also isolate using an EP or 2K filler that is applied in several thin coats, with flash-off times observed.

Most adhesion problems occur when paint fails to stick to the substrate. This is a finishing defect that is perhaps the easiest to avoid. The source of adhesion problems can be one of the following:

  • Improper prep of the substrate
  • Incorrect procedure for prepping plastics
  • Incorrect hardener/thinner combination
  • Incorrect mixing ratio of clearcoat/hardener
  • Basecoat is too thick or not properly dried
  • Intermediate and final flash-off times for the basecoat are too short (basecoat is left too long before top-coating)

Sanding and repainting is the only way to rectify adhesion problems. The issue can be prevented by following the recommendations on the TDS regarding film thickness and intermediate and final flash-off times, as well as clearcoat, hardener and thinner mixtures.


Keeping your paint booth clean and following the recommendations of your paint supplier are the keys to avoiding most finishing defects. If you have questions about how to apply or dry paint, your safest bet is to check with your paint supplier, as a simple phone call could save you a lot of time and expense.

Table of Contents

Related Posts

ā€œI wanted the booth the way I wanted it, and GFS absolutely came throughā€
ā€œThe GFS product line struck me as that cake with whipped cream and not just cakeā€
ā€œWe think the GFS equipment can pay for itself within Year 1ā€
GFS at SEMA 2024: Partnership. Efficiency. Results.
GFS Releases REVO Rapid MC1 Accelerated Curing Technology
Platinum Equipment Named Preferred Global Finishing Solutions Refinish Distributor for Illinois

New Posts

ā€œI wanted the booth the way I wanted it, and GFS absolutely came throughā€
GFS at SEMA 2025: Driven by Performance. Backed by Support.
GFS at FABTECH 2025: Equipment Designed with Finish in Mind
ā€œThe GFS product line struck me as that cake with whipped cream and not just cakeā€
ā€œWe think the GFS equipment can pay for itself within Year 1ā€

Project Profiles

Showcase Your Business

One of the best ways to highlight your business is through a story that you can share across your online platforms. It humanizes your business and shows that your business can make a meaningful impact. Your testimonial would be used as a project profile on the GFS Booth Blog and can be shared on your website and/or social media channels.

Complete this form and we’ll be in touch to showcase your company.

Buy Online for Fast & FREE Shipping

GFS Store Hero image showing BUY NOW items

Shop a variety of GFS aftermarket products, including booth protection products and mobile accelerated curing units. And enjoy the convenience of fast and free ground shipping throughout the contiguous United States.

Center for Excellence facility photo

Located at GFS’ headquarters in Osseo, Wisconsin, the Center for Excellence is an innovative facility featuring an automotive refinish training center, as well as a separate space dedicated to technical product training.

Careers at GFS

Working at GFS Banner image

GFS is continuously searching for talented, ambitious individuals to join our team. We aim to provide our employees with every opportunity to make an impact on the company and find their niche along the way — weather in a production, field services or an office position.Ā 

Sign Up for Our Newsletter
GFS Free Guide Transforming Your Prep Area
Transforming Auto Refinish Prep

Discover the technical advancements that have heightened the importance of the prep area