What You Need to Know to Safely Switch from Solvent-Based to Waterborne Paint

spray gun

As waterborne paint becomes mainstream in the automotive refinish industry and more common for industrial finishing applications, it is crucial to understand how it differs from solvent-based paint, as well as what you need to do to protect your facility and painters.

While the transition from solvent-based paint to waterborne may seem expensive upfront, the costs are justified by creating a healthier work environment for painters, in addition to the environmental benefits. Other perks of waterborne paint include its cleaner, brighter appearance, and ability to more easily color match.

Transitioning to Waterborne

When using waterborne, the paint guns must be made of corrosion-resistant materials. They also must be cleaned with waterborne-specific cleaners, as waterborne paint sticks in places more often than solvent-based paint does. Paint guns designed only for solvent-based paint cannot be used with waterborne.

Curing time for waterborne can be significantly longer than curing time for solvent-based coatings. To avoid a bottleneck in production due to the increased drying time, manufacturing or refinishing processes may need to be adjusted. Options for auto body shops and collision repair centers include AdvanceCure Accelerated Airflow Systems and REVO Accelerated Curing Systems from Global Finishing Solutions (GFS) — time-saving technologies that drastically shorten repair cycle time.

Humidity control is essential with waterborne paint. Unlike solvent-based paint, waterborne does not dry well on its own. Many waterborne paints require a low-humidity environment to assist the drying process. The technical data sheet (TDS) of the coating you are using specifies the desired humidity level. Depending on the humidity level, different additives are required when spraying waterborne. Painters must learn how humidity affects waterborne paint and adjust accordingly. That is why representatives from paint companies typically spend a week or two training painters on how to use waterborne paint.

As you transition to waterborne paint, it may cost less in the long run because less waste is typically created compared to solvent-based paint. Additionally, less product is needed to cover the same area, waterborne paint color matches better and it usually lasts longer in sealed containers, which helps with inventory control.

Paint companies are heavily investing in the development of waterborne. As a result, waterborne has a more vivid hue than solvent-based paint. It also has a high-quality finish, which reduces the required amount of clearcoat.

Less VOCs from Waterborne than Solvent-Based Paint

Volatile organic compounds (VOCs) are carbon-based compounds in solvents that create flammable vapors when evaporated. They contribute to smog and ozone depletion when released directly into the atmosphere, and toxins can persist in the air long after painting is completed. Exposure to VOCs also can cause a range of health problems.

There are fewer solvents in waterborne paint, making it potentially less toxic. However, some solvents are still needed in waterborne paint to achieve the right consistency for application. Conventional basecoats possess a VOC solvent content of about 84 percent, with about 16 percent solids, while waterborne basecoats are comprised of about 70 percent water, about 20 percent solids and about 10 percent solvents.

Since waterborne emits less VOCs than solvent-based paint, air quality is improved and health risks to painters are reduced. It is still important to spray in a high-quality paint booth that meets fire and life safety standards and to always wear the appropriate level of personal protective equipment (PPE).

Fans Are Still Required When Spraying Waterborne Paint

Some may believe that an exhaust fan is not needed in a paint booth when spraying waterborne paint because of the lower emissions of VOCs, but this is not true. A ventless paint booth is not a viable option for containing VOCs or promoting adequate airflow. Even when using waterborne paint, solvents still exist in undercoats and topcoats, so an exhaust fan is needed.

ā€œYou need to have an exhaust fan to remove the flammable or combustible materials,ā€ said Geoff Raifsnider, senior mechanical engineer at GFS. ā€œFlammable or not, overspray is not something you want to be breathing. Plus, you don’t want overspray drifting around the product and landing where you don’t want it to.ā€

Regardless of whether you are spraying waterborne or solvent-based paint, good airflow within the breathing zone — the area immediately in front of a painter — is critical for their health. Downstream of the process, good airflow ensures you avoid high-concentration pockets of vapors that could become ignitable.

ā€œIf you are spraying and light a match in front of the spray gun, you could set the sprayed material on fire. There is a flammable concentration of vapors in the area between you and what you are painting,ā€ Raifsnider said. ā€œThe airflow around you and the piece you are painting dilutes the mists and vapors that are released during the spray process, so that they are not flammable or combustible downstream.ā€

As technology continues to advance, there may come a time when waterborne makes solvent-based paint a thing of the past. If you are new to using waterborne, or even if you have used it for a while, taking the time to educate yourself about the differences from solvent-based paint is essential for the safety of your operation. And whether you are spraying waterborne or solvent-based paint, a proper paint booth is needed to help ensure your facility and painters are protected.

Table of Contents

Related Posts

5 Ways to Keep Your Paint Booth Clean & Operating in Peak Condition
Top 5 Blog Posts of 2020
How to Maximize Your Paint Booth Cycles

New Posts

GFS at SEMA 2025: Driven by Performance. Backed by Support.
GFS at FABTECH 2025: Equipment Designed with Finish in Mind
ā€œThe GFS product line struck me as that cake with whipped cream and not just cakeā€
ā€œWe think the GFS equipment can pay for itself within Year 1ā€
GFS at SEMA 2024: Partnership. Efficiency. Results.

Project Profiles

Showcase Your Business

One of the best ways to highlight your business is through a story that you can share across your online platforms. It humanizes your business and shows that your business can make a meaningful impact. Your testimonial would be used as a project profile on the GFS Booth Blog and can be shared on your website and/or social media channels.

Complete this form and we’ll be in touch to showcase your company.

Buy Online for Fast & FREE Shipping

GFS Store Hero image showing BUY NOW items

Shop a variety of GFS aftermarket products, including booth protection products and mobile accelerated curing units. And enjoy the convenience of fast and free ground shipping throughout the contiguous United States.

Center for Excellence facility photo

Located at GFS’ headquarters in Osseo, Wisconsin, the Center for Excellence is an innovative facility featuring an automotive refinish training center, as well as a separate space dedicated to technical product training.

Careers at GFS

Working at GFS Banner image

GFS is continuously searching for talented, ambitious individuals to join our team. We aim to provide our employees with every opportunity to make an impact on the company and find their niche along the way — weather in a production, field services or an office position.Ā 

Sign Up for Our Newsletter
GFS Free Guide Transforming Your Prep Area
Transforming Auto Refinish Prep

Discover the technical advancements that have heightened the importance of the prep area