Your Questions, Answered — Paint Booth Pressure Gauges

Q: Are manometers or other pressure-drop devices required by law on exhaust filters?

A: A means is required to make sure that you are moving the required amount of air for paint spraying. Your choices depend upon the code or standard adopted by your local authority. According to the NFPA® 1 Fire Code, the requirements spelled out in NFPA® 33 Standard for Spray Application Using Flammable or Combustible Materials 2011 Edition would apply.

NFPA 33 states that Spray areas equipped with overspray collection filters shall have an effective means to ensure that the performance requirements of Section 7.2 are met.” [33:7.2.1] NFPA 33 also offer explanatory material that says that “Acceptable means to comply with 7.2.1 include, but are not limited to, visible gauges, audible alarms, approved interlocks, or an effective inspection program.” [33:A7.2.1] says that “Acceptable means to comply with 7.2.1 include, but are not limited to, visible gauges, audible alarms, approved interlocks, or an effective inspection program.” [33:A7.2.1]

According to the International Fire Code, the requirements spelled out in Chapter 24 would apply. The IFC states that “Visible gauges, audible alarms or pressure-activated devices shall be installed to indicate or ensure that the required air velocity is maintained.” [IFC:2404.7.8.3]

Therefore, some means is required to ensure that the required air movement is maintained within the spray area. Both codes give you options. The intent of these requirements is to alert the operator of the point where the filters are loaded and can no longer pass the required amount of air. At that point, the filters need to be replaced.

Pressure Gauges

Q: What is the best placement of the sensor tubes coming from the magnahelic gauge for a downdraft pit type booth?

A: The answer depends on what pressure differential you are trying to measure. If you are measuring cabin pressure compared to building pressure, the high pressure sensor tube should be mounted in the cabin away from any booth openings. The low pressure tube should be left open to the shop. If you want to measure static pressure loss across the pit filter, the high pressure sensor tube should be mounted in the cabin away from any booth openings, and the low pressure sensor a few inches below the pit filters.

Table of Contents

Related Posts

“I wanted the booth the way I wanted it, and GFS absolutely came through”
Ultra XS Paint Booth a “Wow Factor” for Ministry Helping At-Risk Teens
“Potential is There for More Throughput” with Dual-Bay CTOF Booth at ABRA Faribault
Share the Filtered Air: Community Paint Booth a Clean Space for Ohio Woodworkers
Beating the Heat: “There are no temperature swings” in Ultra Paint Booths
Not a Small World: Large Equipment Paint Booth Has Camping World of Madison Thinking Big

New Posts

“I wanted the booth the way I wanted it, and GFS absolutely came through”
GFS at SEMA 2025: Driven by Performance. Backed by Support.
GFS at FABTECH 2025: Equipment Designed with Finish in Mind
“The GFS product line struck me as that cake with whipped cream and not just cake”
“We think the GFS equipment can pay for itself within Year 1”

Project Profiles

Showcase Your Business

One of the best ways to highlight your business is through a story that you can share across your online platforms. It humanizes your business and shows that your business can make a meaningful impact. Your testimonial would be used as a project profile on the GFS Booth Blog and can be shared on your website and/or social media channels.

Complete this form and we’ll be in touch to showcase your company.

Buy Online for Fast & FREE Shipping

GFS Store Hero image showing BUY NOW items

Shop a variety of GFS aftermarket products, including booth protection products and mobile accelerated curing units. And enjoy the convenience of fast and free ground shipping throughout the contiguous United States.

Center for Excellence facility photo

Located at GFS’ headquarters in Osseo, Wisconsin, the Center for Excellence is an innovative facility featuring an automotive refinish training center, as well as a separate space dedicated to technical product training.

Careers at GFS

Working at GFS Banner image

GFS is continuously searching for talented, ambitious individuals to join our team. We aim to provide our employees with every opportunity to make an impact on the company and find their niche along the way — weather in a production, field services or an office position. 

Sign Up for Our Newsletter
GFS Free Guide Transforming Your Prep Area
Transforming Auto Refinish Prep

Discover the technical advancements that have heightened the importance of the prep area